Email Us
BYP17 (4J33) Controlled-Expansion Alloy
Overview of BYP17 (4J33) Controlled-Expansion Alloy
Request A Quote +

BYP17 (4J33) has a similar linear expansion coefficient with 95% Al2O3 ceramics from -60℃ to 600℃. This makes it a reliable solution for high-reliability sealing and bonding, a performance hallmark of premium controlled expansion alloys and a sought-after property in the broader thermal expansion alloys category.


invar thermal expansion BYP17 4J33 Controlled Expansion Alloy

The Typical Applications of This Alloy are

  • Sealing between vacuum tubes and 95% Al2O3 ceramics


Typical Chemical Composition in Percent


Ni

32.1~33.6

Fe

bal.

Co

14.0~15.2





Typical Linear Expansion Coefficient


25℃-400℃

6.0~6.8

25℃-500℃

6.6~7.4



Typical Mechanical Properties

Tensile Strength

Soft

Hard


<570 MPa (82.7 ksi)

>700 Mpa (101.5 ksi)

Hardness

Thickness

Deep-drawing State


>0.2~2.5mm

≤165HV


>2.5mm

≤170HV

Gain Size

Deep-drawing State: ≥Level 7



Feel free to reach out to Beiye for a quote on BYP17 (4J33) and our comprehensive precision alloy and supply services.


Thank You for Your Attention on Beiye!
Thank You for Your Attention on Beiye!
Contact Us
Add:
No.1, Qinghe Xiaoying East Road, Haidian District, Beijing City, P.R. China
Build the Future with Steel
Add:
No.1, Qinghe Xiaoying East Road, Haidian District, Beijing City, P.R. China