Email Us
BYP12 (4J29) Controlled-Expansion Alloy
Overview of BYP12 (4J29) Controlled-Expansion Alloy
Request A Quote +

BYP12 (4J29) has a certain linear expansion coefficient from -60℃ to 400℃. Similar alloy's names in different trademark systems:

Beiye

China Standard

America

Germany

France

Japan

BYP12

4J29

AMS7727A

AMS7728E

Class1

Ni29Co18

Fe-Ni29Co17

Fe-Ni-Co sealing alloy



invar thermal expansion

The Typical Applications of This Alloy are

  • Sealing alloys for hard glasses

  • Transmitting tube

  • Oscillation tube

  • Ignitron

  • Transistor

  • Relay shell


Typical Chemical Composition in Percent


Ni

28.5~29.5

Fe

bal.

Co

16.8~17.8





Typical Linear Expansion Coefficient


25℃-400℃

4.6~5.2

25℃-450℃

5.1~5.5



Typical Mechanical Properties


Tensile Strength





Soft

1/4Hard

1/2Hard

3/4Hard

Hard

<570 MPa

(82.7 ksi)

520~630 MPa

(75.4~91.4 ksi)

590~700 MPa

(85.6~101.5 ksi)

600~770 MPa

(87.0~111.7 ksi)

>700 MPa

(>101.5ksi)

Hardness

Thickness

Deep-drawing State


>0.2~2.5mm

≤165HV


>2.5mm

≤170HV

Gain Size

Deep-drawing State: ≥Level 7




Typical Physical Properties

Density

8.17 g/cm3 (0.298 lb/in3)

Resistivity

46 µΩ•cm

Thermal conduction

19 W/K

Elastic modulus

134 Gpa



Thank You for Your Attention on Beiye!
Thank You for Your Attention on Beiye!
Contact Us