1.4957 Cast Superalloy
Overview of 1.4957 Cast Superalloy
Request A Quote +

1.4957 is a kind of iron - nickel -molybdenum austenitic heat resisting steels alloy which has high performance cast material for high temperature applications. Manufacturing a high-integrity castalloy factory product like this is a core competency of premier super alloy manufacturers. 

Beiye designationChina Standard designationInternational designation

1.4957

/

1.4957, GX 15CrNiCo212020



co cr ni alloy 1 4957

The Typical Applications of This Alloy are

  • Turbocharger components like bushings, e.g. Wastegate-turbochargers


Typical Chemical Composition in Percent


C

0.17

Ni

20

Cr

21

Si

0.6

Mo

3



W

2.8

Nb

1.1



Co

20

N

0.16



Mn

1.7

Febal.



Typical Mechanical Properties



As  cast

Yield Strength

345 MPa

Tensile Strength

655MPa

Elongation

25%


* Typical values for material tested in accordance with GB/T 228, GB/T 22315.


Typical Physical Properties


Density

8.25g/cm3

Melting Point

1350 ℃

Thermal expansion(20~1000℃)

18×10-6/K

As a leader in this field, Beiye has built a robust system for precision alloy and supply, guaranteeing that every batch meets stringent specifications for critical high-temperature environments.


Heat Treatment

Heat treatment not allowed.


Thank You for Your Attention on Beiye!
Thank You for Your Attention on Beiye!
Contact Us
Add:
No.1, Qinghe Xiaoying East Road, Haidian District, Beijing City, P.R. China
Build the Future with Steel
Add:
No.1, Qinghe Xiaoying East Road, Haidian District, Beijing City, P.R. China