HIT3312 is a kind of iron - nickel -molybdenum austenitic heat resisting steels alloy which has high performance cast material for high temperature applications. The performance of this advanced cast alloy in critical situations depends heavily on the reliability of your super alloy suppliers.
| Beiye designation | China Standard designation | International designation |
| ST33-12,HIT3312 | / | GX30CrNiMo26-20-2 |
| The typical applications of this alloy are: | ||
| turbocharger components like bushings, e.g. Wastegate-turbochargers. | ||
Turbocharger components like bushings, e.g. Wastegate-turbochargers.
C | 0.3 | Ni | 18.5 |
| Si | 2.7 | Mo | 2.5 |
| W | 2.6 | Nb | 1.4 |
| S | 0.3 | N | 0.24 |
| Mn | 1.4 | Fe | bal. |
As cast | |
Hardness | 230 to 360 HV |
* Typical values for material tested in accordance with GB/T 4340.3
| Density | 8.15g/cm3 |
Melting Point | 1360 ℃ |
Thermal expansion(20~1000℃) | 18×10-6/K |
As a industry-recognized leader, Beiye provides a fully integrated precision alloy and supply service to ensure material integrity from production to delivery.
Heat treatment not allowed.